Asaclean® Purging Instructions for Shutdown/Start-up of High Heat Resins Using PX2 Grade (Above 360ºC, 680ºF)
Shutdown
- Upon completion of molding or extrusion run, purge the machine with Asaclean® PX2 following the standard purging procedures.
- Purging out of the first resin should be completed prior to dropping the temperatures to 280ºC (535ºF). The barrel should be left full of Asaclean® to prevent the entry of oxygen into the barrel that will accelerate material decomposition and carbon formation. Asaclean® PX2 should not be left idle in the machine for ANY period of time at ANY temperature.
- Continuously displace the PX2 with a fresh barrel capacity of PX2 and continue to decrease temperatures. Before 280ºC (535ºF) is reached, displace PX2 with a nonglass filled grade of Asaclean® (U, UP, or E). When all of the PX2 Grade has been removed, ensure that the barrel is full of the non-glass filled Asaclean® grade and turn off heaters.
- Do not allow the temperatures in the barrel to drop below 280ºC (535ºF) with Asaclean® PX2 in the barrel as overloading of the screw may occur during rotation.
Start-up
- Turn on the heaters and wait until the temperature of Asaclean® in the barrel reaches 280ºC (535ºF). Allow adequate time for all of the Asaclean® to plasticize, including material far from the thermocouple at the barrel wall, before turning the screw (to prevent damage).
- For injection molding: with maximum safe back pressure and the screw completely forward, start feeding PX2 Grade to displace the non-glass filled Asaclean® grade after temperatures are above 280°C (535°F). (Do not allow the temperatures in the barrel to drop below 280ºC (535ºF) with Asaclean® PX2 in the barrel as overloading of the screw may occur during rotation.)
- When PX2 comes out from the nozzle or die, increase the screw speed to maximum safe level.
- Continue to increase the temperature in the barrel to the processing range of the high heat resin. Asaclean® PX2 should not be left idle in the machine for ANY period of time at ANY temperature.
- Begin feeding the next resin.
- For injection molding: Use maximum safe back pressure and screw speed until the next resin starts coming out from the nozzle and all of the Asaclean® is displaced. For extrusion: Use maximum safe screw speed until all of the Asaclean® is displaced.
- Begin production under normal processing conditions for the next resin.
Technical questions?
To request detailed technical bulletins or technical support, contact us at Asahi Kasei Plastics North America Inc.
Phone: (800) 787-4348 / (973)257-1999
Fax: (973) 257-1011
Website: www.Asaclean.com
E-mail: sales@Asaclean.com